INEOS Styrolution Terlux HD 2802透明医疗级ABS
Density | 1.08 | g/cm³ | *** 1183 |
Apparent (Bulk) Density 3 | 0.59 | g/cm³ | |
Melt Volume-Flow Rate (MVR) | *** 1133 | ||
220°C/10.0 kg | 2.0 | cm³/10min | |
220°C/21.6 kg | 17 | cm³/10min | |
Molding Shrinkage | 0.40 to 0.70 | % | *** 294-4 |
Water Absorption (Saturation, 23°C) | 0.70 | % | *** 62 |
Hardness | Nominal Value | Unit | Test Method |
Ball Indentation Hardness | 70.0 | MPa | *** 2039-1 |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 2000 | MPa | *** 527-1 |
Tensile Stress (Yield, 23°C) | 48.0 | MPa | *** 527-2 |
Tensile Strain (Yield, 23°C) | 4.0 | % | *** 527-2 |
Nominal Tensile Strain at Break (23°C) | 12 | % | *** 527-2 |
Tensile Creep Modulus (1000 hr) | 1250 | MPa | *** 899-1 |
Flexural Stress (23°C) | 70.0 | MPa | *** 178 |
Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength | *** 179/1eA | ||
-30°C | 2.0 | kJ/m² | |
23°C | 5.0 | kJ/m² | |
Charpy Unnotched Impact Strength | *** 179/1eU | ||
-30°C | 80 | kJ/m² | |
23°C | 120 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load 4 | |||
0.45 MPa, Annealed | 94.0 | °C | *** 75-2/B |
1.8 MPa, Annealed | 90.0 | °C | *** 75-2/A |
Vicat Softening Temperature | |||
-- | 93.0 | °C | *** 306/B50 |
-- | 105 | °C | *** 306/A50 |
CLTE - Flow | 8.0E-5 to 1.1E-4 | cm/cm/°C | *** 11359-2 |
Thermal Conductivity | 0.17 | W/m/K | DIN 52612 |