INCONEL® alloy 625LCF (UNS N06626 / W. Nr. 2.4856) was developed as a fatigue-resistant, bellows-quality version of INCONEL alloy 625. Alloying, melting and processing are designed and controlled to provide a sheet product with optimum resistance to low-cycle and thermal fatigue at up to 1200°F (650°C). The alloy offers a highlevel of performance in aircraft exhaust and automotive flexible coupling bellows, expansion joints in process or transport piping, and other applications involving resistance to low-cycle or thermal fatigue. INCONEL alloy 625LCF is covered by U.S patent 4,765,956. Table 1 - Limiting Chemical Composition, wt %* *UNS N06626 a Plus Ta.ªMean coefficient of linear expansion between 70°F (21°C) and temperature shown. Nickel..........................................................................58.0 min.Chromium..................................................................20.0-23.0 Molybdenum................................................................8.0-10.0 Niobiuma .....................................................................3.15-4.15 Iron...............................................................................5.0 max. Carbon.......................................................................0.03 max. Manganese................................................................0.50 max. Silicon........................................................................0.15 max. Sulfur........................................................................0.015 max. Aluminum...................................................................0.40 max. Titanium ....................................................................0.40 max. Phosphorus.............................................................0.015 max. Cobalt.........................................................................1.0 max. Nitrogen....... ...........................................................0.02 max.
Inconel625,NS336,UNS N06625,Alloy625,2.4856,NCF625供应商
Inconel625,NS336,UNS N06625,Alloy625,2.4856,NCF625物理性能:
密度: 8.44g/cm3 熔点:1290-1350 °C
弹性模量: 205.8N/mm2 热导率:19.8 W/m•K
硬度:HBS(187-217) 热膨胀系数( 21 - 93°C): 12.8 μ m/m °C
Inconel 625合金的主要化学成分如下:C≤0.10 Si≤0.5 Mn≤0.50 S≤0.015 P≤0.015 Ni≥58.0 Cr=20.0~23.0 Fe≤5.0 Al≤0.4 Mo=8.0~10.0 Nb=3.15~4.15 Ti≤0.40 Co≤1.0
品种规格有:锻件、棒材、板材、带材、环件、丝材、螺栓、弹簧等协商供应,可根据客户要求生产。
欢迎新老客户来电洽谈咨询,
联系方式:
联系人:罗经理
手机: 13671561267
电话: 021-54461707/021-54192998-618
传真: 021-54192997
QQ: 279851675
邮箱: 279851675@qq.com
上海宝缘钢铁有限公司生产供应NS336(inconel625),无缝钢管、圆钢、管件、锻件、法兰、焊丝、配件等,并可定做各种非标材料。NS336(Inconel 625) 是一种镍铬钼合金,还有少量铌,用以加强合金的硬度,因此此合金不需要热处理就能增加很高的强度.此合金可以在很多种严酷的酸性环境中抵御腐蚀,特别是***腐蚀及裂隙腐蚀.运用于化学加工,航空领域,轮机引擎,污染控制设备,和核反应设备。
Inconel 625
1. 特性
该合金属于镍铬钼铌系镍基耐蚀,耐热固溶强化变形合金。
在650°C 以下具有优良的持久性能,疲劳性能,耐腐蚀和抗氧化性能。
由于含有较高的合金元素,能耐各种各样的腐蚀环境,能抗氯离子应力腐蚀裂纹。 该合金具有优良的耐点腐蚀性能和耐间隙腐蚀性能。
2. 化学成分(%)
Ni Nb(+Ta) Si Cr C S Mo Mn Fe Al Ti P Co
》58.0 3.15/4.15 《0.50 20.0-23.0 《0.10 《0.015 8.0-10.0 《0.5 《5.0 《0.40 《0.40 《0.015 《1.0
3. 机械性能
屈服强度 Mpa 抗拉强度 Mpa 延长率 (%)
》380 》830 》30
4. 物理性能
密度: 8.44 g/cm3 熔点: 1219-1350 °C
比热: 410 J/kg · °C 电阻率: 1.29 µΩ· m
5. 应用
软化退火后的低碳合金625广泛的应用于化工流程工业,较好的耐腐蚀性和高强度使之能作为较薄的结构部件。625合金可以应用于接触海水并承受高机械应力的场合。典型应用领域:
1.含氯化物的有机化学流程工艺的部件,尤其是在使用酸性氯化物催化剂的场合
2.用于制造纸浆和造纸工业的蒸煮器和漂白池
3.烟气脱硫系统中的吸收塔、再加热器、烟气进口挡板、风扇(潮湿)、搅拌器、导流板以及烟道等
4.用于制造应用于酸性气体环境的设备和部件
5.乙酸和乙酐反应发生器
6.硫酸冷凝器
Inconel625,NS336,UNS N06625,Alloy625,2.4856,NCF625供应商
Inconel625,NS336,UNS N06625,Alloy625,2.4856,NCF625物理性能:
密度: 8.44g/cm3 熔点:1290-1350 °C
弹性模量: 205.8N/mm2 热导率:19.8 W/m•K
硬度:HBS(187-217) 热膨胀系数( 21 - 93°C): 12.8 μ m/m °C
Inconel 625合金的主要化学成分如下:C≤0.10 Si≤0.5 Mn≤0.50 S≤0.015 P≤0.015 Ni≥58.0 Cr=20.0~23.0 Fe≤5.0 Al≤0.4 Mo=8.0~10.0 Nb=3.15~4.15 Ti≤0.40 Co≤1.0
品种规格有:锻件、棒材、板材、带材、环件、丝材、螺栓、弹簧等协商供应,可根据客户要求生产。
欢迎新老客户来电洽谈咨询,