导电高抗冲POM Hostaform EC270TX Celanese
Density | 1.38 | g/cm³ | *** 1183 |
Melt Volume-Flow Rate (MVR) (190°C/2.16 kg) | 1.5 | cm³/10min | *** 1133 |
Molding Shrinkage | *** 294-4 | ||
Across Flow | 1.7 | % | |
Flow | 1.9 | % |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 1950 | MPa | *** 527-1 |
Tensile Stress (Yield) | 44.0 | MPa | *** 527-2/50 |
Tensile Strain (Yield) | 11 | % | *** 527-2/50 |
Nominal Tensile Strain at Break | 15 | % | *** 527-2/50 |
Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength (23°C) | 6.5 | kJ/m² | *** 179/1eA |
Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 70.0 | °C | *** 75-2/A |
Melting Temperature 3 | 166 | °C | *** 11357-3 |
Electrical | Nominal Value | Unit | Test Method |
Surface Resistivity (23°C) | 1.0E+3 | ohms | IEC 62631-3-2 |
Volume Resistivity (23°C) | 10 | ohms·m | IEC 62631-3-1 |