| 性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 | |
| 机械性能 | 拉伸强度(引张强度) | ASTM D638/*** 527 | 290 屈服 200断裂 | kg/cm²(MPa)[Lb/in2] | |
| 断裂伸长率 | ASTM D638/*** 527 | >300 | % | ||
| 拉伸模量 | ASTM D638/*** 527 | kg/cm²(MPa)[Lb/in2] | |||
| 拉伸屈服伸长率(延伸率) | ASTM D638/*** 527 | % | |||
| 拉伸断裂伸长率(延伸率) | ASTM D638/*** 527 | % | |||
| 弯曲模量(弯曲弹性率) | ASTM D790/*** 178 | 13000 | kg/cm²(MPa)[Lb/in2] | ||
| 弯曲强度 | ASTM D790/*** 178 | kg/cm²(MPa)[Lb/in2] | |||
| 洛氏硬度 | ASTM D785 | R-82 | |||
| IZOD 缺口冲击强度 | 1/4" 23℃ | ASTM D256/*** 179 | 12 | kg·cm/cm(J/M)ft·lb/in | |
| 1/4" -30℃ | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" 23℃ | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 1/8" -30℃ | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| Charpy冲击强度 | 23℃ (缺口) | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | ||
| -30℃(缺口) | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 23℃(无缺口) | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| -30℃(无缺口) | ASTM D256/*** 179 | kg·cm/cm(J/M)ft·lb/in | |||
| 物性性能 | 比重(密度) | ASTM D792/*** 1183 | 0.91 | ||
| 成型收缩率 | ASTM D955 | % | |||
| 熔融指数(流动系数) | 200℃/5kg | ASTM D1238/*** 1133 | 5 | g/10min | |
| 220℃/10kg | ASTM D1238/*** 1133 | g/10min | |||
| 吸水率 23℃/24H | ASTM D570/*** 62 | % | |||
| 热性能 | 热变形温度 | 退火 | ASTM D648/*** 75 | 110 | ℃(℉) |
| 未退火 | ASTM D648/*** 75 | ℃(℉) | |||
| 维卡软化点 | ASTM D1525/*** R306 | 152 | ℃(℉) | ||