直销北欧化工20%MF增强PP Borealis ME212U
Density | 1.05 | g/cm³ | *** 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 13 | g/10 min | *** 1133 |
Molding Shrinkage | 1.2 | % | Internal Method |
| Hardness | Nominal Value | Unit | Test Method |
Ball Indentation Hardness (H 358/30) | 96.0 | MPa | *** 2039-1 |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus (Injection Molded) | 2900 | MPa | *** 527-2/1 |
Tensile Stress (Yield, Injection Molded) | 32.0 | MPa | *** 527-2/50 |
Tensile Strain (Yield, Injection Molded) | 10 | % | *** 527-2/50 |
Flexural Modulus 3 (Injection Molded) | 3100 | MPa | *** 178 |
Flexural Stress (Injection Molded) | 50.0 | MPa | *** 178 |
| Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength | *** 179/1eA | ||
-20°C | 1.5 | kJ/m² | |
23°C | 3.0 | kJ/m² | |
Charpy Unnotched Impact Strength | *** 179/1eU | ||
-20°C | 15 | kJ/m² | |
23°C | 35 | kJ/m² | |
Notched Izod Impact Strength | *** 180/1A | ||
-20°C | 2.0 | kJ/m² | |
23°C | 3.5 | kJ/m² | |
Unnotched Izod Impact Strength | *** 180/1U | ||
-20°C | 15 | kJ/m² | |
23°C | 40 | kJ/m² |