Density | 0.900 | g/cm³ | ExxonMobil Method |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 4.0 | g/10 min | ASTM D1238 |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Strength | |||
Yield 3 | 25.2 | MPa | ASTM D638 |
Yield | 24.6 | MPa | *** 527-2/50 |
Tensile Elongation | |||
Yield 3 | 5.3 | % | ASTM D638 |
Yield | 4.7 | % | *** 527-2/50 |
Flexural Modulus | |||
1% Secant 4 | 1380 | MPa | ASTM D790A |
1% Secant 5 | 1510 | MPa | ASTM D790B |
-- 6 | 1360 | MPa | *** 178 |
| Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength | *** 179/1eA | ||
-20°C | 7.7 | kJ/m² | |
23°C | 55 | kJ/m² | |
Notched Izod Impact | |||
-18°C | 80 | J/m | ASTM D256A |
23°C | No Break | ASTM D256A | |
-40°C | 7.7 | kJ/m² | *** 180/1A |
-18°C | 9.2 | kJ/m² | *** 180/1A |
23°C | 52 | kJ/m² | *** 180/1A |
Gardner Impact 7 (-29°C, 3.18 mm) | 26.1 | J | ASTM D5420 |
| Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load | |||
0.45 MPa, Unannealed | 106 | °C | ASTM D648 |
0.45 MPa, Unannealed | 95.7 | °C | *** 75-2/Bf |
1.8 MPa, Unannealed | 51.4 | °C | *** 75-2/Af |