***美国SABIC高CT***PPO NORYL NH6020
Density / Specific Gravity | 1.14 | g/cm | ASTM D792,*** 1183 |
Melt Mass-Flow Rate (MFR)(280°C/5.0 kg) | 14 | g/10 min | ASTM D1238 |
Melt Volume-Flow Rate (MVR)(280°C/5.0 kg) | 11 | cm/10min | *** 1133 |
Molding Shrinkage - Flow(3.20 mm) | 0.50 to 0.70 | % | Internal Method |
Water Absorption |
|
| *** 62 |
Saturation, 23°C | 0.18 | % |
|
Equilibrium, 23°C, 50% RH | 0.060 | % |
|
Outdoor Suitability | f1 |
| UL 746C |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus |
|
|
|
--2 | 2740 | MPa | ASTM D638 |
-- | 2740 | MPa | *** 527-2/1 |
Charpy Notched Impact Strength7(23°C) | 9.0 | kJ/m | *** 179/1eA |
Notched Izod Impact |
|
|
|
-30°C | 36 | J/m | ASTM D256 |
23°C | 49 | J/m | ASTM D256 |
-30°C8 | 5.0 | kJ/m | *** 180/1A |
23°C8 | 8.0 | kJ/m | *** 180/1A |
Instrumented Dart Impact(23°C, Total Energy) | 18.0 | J | ASTM D3763 |