日本油墨PPS FZ-2140-B2高流动40%GF
| 物理性能 | 比重 | ASTMD792 | 1.66 | g/cm | |
| 收缩率 | 流动 | ASTMD955 | 0.25 | % | |
| 横向流动 | ASTMD955 | 1.1 | % | ||
| 吸水率(23°C,24hr) | ASTMD570 | 0.020 | % | ||
| 硬度 | 洛氏硬度 | M级 | ASTMD785 | 100 | |
| R级 | ASTMD785 | 121 | |||
| 机械性能 | 拉伸模量 | ASTMD638 | 14000 | MPa | |
| 抗张强度 | ASTMD638 | 180 | MPa | ||
| 伸长率(断裂) | ASTMD638 | 1.8 | % | ||
| 弯曲模量 | ASTMD790 | 13000 | MPa | ||
| 弯曲强度 | ASTMD790 | 270 | MPa | ||
| 压缩强度 | ASTMD695 | 200 | MPa | ||
| 泊松比 | 0.36 | ||||
| 摩擦系数3 | 与钢-动态 | ASTMD1894 | 0.35 | ||
| 与钢-静态 | ASTMD1894 | 0.35 | |||
| 断裂弯曲伸长率 | ASTMD790 | 2.5 | % | ||
| 冲击性能 | 悬壁梁缺口冲击强度 | ASTMD256 | 100 | J/m | |
| 无缺口悬臂梁冲击 | ASTMD256 | 550 | J/m | ||
| 热性能 | 载荷下热变形温度(1.8MPa,未退火) | ASTMD648 | 265 | °C | |
| 线形热膨胀系数 | 流动:-30到90°C | ASTMD696 | 2.2E-5 | cm/cm/°C | |
| 横向:-30到90°C | ASTMD696 | 2.2E-5 | cm/cm/°C | ||
| 电气性能 | 体积电阻率 | ASTMD257 | 1.0E+16 | ohms·cm | |
| 介电强度(1.60mm) | ASTMD149 | 16 | kV/mm | ||
| 介电常数(1MHz) | ASTMD150 | 4.00 | |||
| 耗散因数(1MHz) | ASTMD150 | 2.0E-3 | |||
| 耐电弧性 | ASTMD495 | 125 | sec | ||
| 漏电起痕指数 | ASTMD3638 | 170 | V | ||
| 可燃性 | UL阻燃等级(0.8mm) | UL94 | V-0 |
PPS是一种综合性能***的热塑性特种工程塑料,其突出的特点是***,***和优越的机械性能。PPS是含硫芳香族聚合物,线型PPS在350℃以上交联后成热固性塑料,支链型结构PPS为热塑性塑料。PPS是美国菲利普斯公司于1971年首先实现工业化生产的,***到期后,日本的企业也开始研发和生产。日企比较典型的有日本的东丽公司,现阶段日本的产量已大于美国的产量。其他一些生产厂家也主要集中在美国,日本,欧洲。
在线问