Surlyn® 8940-E
离聚物
DuPont Packaging & Industrial Polymers
产品说明:
Surlyn® 8940-E is a sodium ionomer thermoplasic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shape.
Surlyn® 8940-E thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions.
Surlyn® 8940-E 物性表
物理性能 | 额定值 | 单位制 | 测试方法 |
---|
比重 | 0.950 | g/cm³ | ASTM D792, *** 1183 |
熔流率(熔体流动速率) (190°C/2.16 kg) | 2.8 | g/10 min | ASTM D1238, *** 1133 |
硬度 | 额定值 | 单位制 | 测试方法 |
---|
肖氏硬度 (邵氏 D) | 65 |
| ASTM D2240, *** 868 |
机械性能 | 额定值 | 单位制 | 测试方法 |
---|
抗张强度 |
|
| ASTM D638, *** 527-2 |
屈服, 23°C | 15.0 | MPa | ASTM D638, *** 527-2 |
断裂, 23°C | 33.0 | MPa | ASTM D638, *** 527-2 |
伸长率 (断裂, 23°C) | 470 | % | ASTM D638, *** 527-2 |
弯曲模量 |
|
| ASTM D790 |
-20°C | 717 | MPa | ASTM D790 |
23°C | 350 | MPa | ASTM D790 |
抗磨损性 - NBS Index | 370 |
| ASTM D1630 |
热性能 | 额定值 | 单位制 | 测试方法 |
---|
Freezing Point | 59 | °C | ASTM D3418 |
弹性体 | 额定值 | 单位制 | 测试方法 |
---|
撕裂强度 (23°C) | 1.48 | kN/m | ASTM D624 |
冲击性能 | 额定值 | 单位制 | 测试方法 |
---|
悬壁梁缺口冲击强度 (23°C) | 1000 | J/m | ASTM D256 |
拉伸冲击强度 |
|
| ASTM D1822 |
-40°C | 757 | kJ/m² | ASTM D1822 |
23°C | 1020 | kJ/m² | ASTM D1822 |
热性能 | 额定值 | 单位制 | 测试方法 |
---|
脆化温度 | -106 | °C | ASTM D746 |
维卡软化温度 | 63.0 | °C | ASTM D1525, *** 306 |
熔融峰值温度 | 94.0 | °C | ASTM D3418, *** 3146 |
光学性能 | 额定值 | 单位制 | 测试方法 |
---|
雾度 (6350 µm) | 5.0 | % | ASTM D1003 |
注射 | 额定值 | 单位制 |
|
---|
加工(熔体)温度 | 185 到 285 | °C |
|