原包美国SABIC无卤阻燃PPO NORYL N1250
Density / Specific Gravity | 1.10 | g/cm | ASTM D792 |
Melt Mass-Flow Rate (MFR)(300°C/5.0 kg) | 28 | g/10 min | ASTM D1238 |
Molding Shrinkage - Flow(3.20 mm) | 0.50 to 0.70 | % | Internal Method |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus2 | 2700 | MPa | ASTM D638 |
Tensile Strength3 |
|
| ASTM D638 |
Yield | 77.0 | MPa |
|
Break | 62.0 | MPa |
|
Tensile Elongation3 |
|
| ASTM D638 |
Yield | 5.0 | % |
|
Break | 15 | % |
|
Flexural Modulus4(50.0 mm Span) | 2800 | MPa | ASTM D790 |
Flexural Strength4(Yield, 50.0 mm Span) | 120 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
Notched Izod Impact(23°C) | 100 | J/m | ASTM D256 |
Instrumented Dart Impact(23°C, Total Energy) | 40.0 | J | ASTM D3763 |