日本东丽40%GF低毛边PPS TORELINA A504X95
Density(23°C) | 1.66 | g/cm | *** 1183 |
Molding Shrinkage3 |
|
| Internal Method |
Across Flow : 3.00 mm | 0.80 | % |
|
Flow : 3.00 mm | 0.20 | % |
|
Water Absorption(24 hr, 23°C) | 0.020 | % | *** 62 |
| Hardness | Nominal Value | Unit | Test Method |
Rockwell Hardness(R-Scale) | 122 |
| *** 2039-2 |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Stress(23°C) | 200 | MPa | *** 527-2 |
Tensile Strain(Break, 23°C) | 1.6 | % | *** 527-2 |
Flexural Modulus(23°C) | 15500 | MPa | *** 178 |
Flexural Stress(23°C) | 290 | MPa | *** 178 |
Shear Strength(23°C) | 75.0 | MPa | JIS K7214 |
Coefficient of Friction4 | 0.25 |
|
|
Taber Abrasion Resistance(1000 Cycles) | 50.0 | mg | *** 9352 |
| Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength(23°C) | 11 | kJ/m | *** 179 |
Charpy Unnotched Impact Strength(23°C) | 45 | kJ/m | *** 179 |
| Thermal | Nominal Value | Unit | Test Method |
Heat Deflection Temperature(1.8 MPa, Unannealed) | 260 | °C | *** 75-2/A |
Melting Temperature | 278 | °C | *** 11357-3 |
CLTE |
|
| *** 11359-2 |
Flow | 2.3E-5 | cm/cm/°C |
|
Transverse | 3.1E-5 | cm/cm/°C |
|
| Electrical | Nominal Value | Unit | Test Method |
Volume Resistivity | 1.0E+14 | ohms·cm | IEC 60093 |
Electric Strength | 25 | kV/mm | IEC 60243-1 |
Dielectric Constant5(23°C, 1 MHz) | 3.60 |
| IEC 60250 |
Dissipation Factor5(23°C, 1 MHz) | 2.0E-3 |
| IEC 60250 |
| Flammability | Nominal Value | Unit | Test Method |
Flame Rating(0.28 mm) | V-0 |
| UL 94 |
PPS是一种综合性能***的热塑性特种工程塑料,其突出的特点是***,***和优越的机械性能。PPS是含硫芳香族聚合物,线型PPS在350℃以上交联后成热固性塑料,支链型结构PPS为热塑性塑料。PPS是美国菲利普斯公司于1971年首先实现工业化生产的,***到期后,日本的企业也开始研发和生产。日企比较典型的有日本的东丽公司,现阶段日本的产量已大于美国的产量。其他一些生产厂家也主要集中在美国,日本,欧洲。