日本油墨40%玻纤低毛边PPS FZ-1140-D5
Density / Specific Gravity | 1.66 | g/cm | ASTM D792 |
Molding Shrinkage |
|
| ASTM D955 |
Flow | 0.25 | % |
|
Across Flow | 1.1 | % |
|
Water Absorption(24 hr, 23°C) | 0.020 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
Rockwell Hardness |
|
| ASTM D785 |
M-Scale | 100 |
|
|
R-Scale | 121 |
|
|
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 15000 | MPa | ASTM D638 |
Tensile Strength | 190 | MPa | ASTM D638 |
Tensile Elongation(Break) | 1.8 | % | ASTM D638 |
Flexural Modulus | 13500 | MPa | ASTM D790 |
Flexural Strength | 270 | MPa | ASTM D790 |
Flexural Elongation (Break) | 2.5 | % | ASTM D790 |
Compressive Strength | 200 | MPa | ASTM D695 |
Poisson's Ratio | 0.36 |
|
|
Coefficient of Friction3 |
|
| ASTM D1894 |
vs. Steel - Dynamic | 0.35 |
|
|
vs. Steel - Static | 0.35 |
|
|
| Impact | Nominal Value | Unit | Test Method |
Notched Izod Impact | 100 | J/m | ASTM D256 |
Unnotched Izod Impact | 600 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load(1.8 MPa, Unannealed) | 265 | °C | ASTM D648 |
CLTE |
|
| ASTM D696 |
Flow : -30 to 90°C | 2.2E-5 | cm/cm/°C |
|
Transverse : -30 to 90°C | 2.2E-5 | cm/cm/°C |
|
PPS在负荷下的耐蠕变性好,硬度高;***性高,其1000转时的磨耗量仅为0.04g,填充F4及二硫化钼后还会进一步得到改善;PPS还具有一定的自润性。PPS的机械性能对温度的敏感性能小(3)热学性能:PPS具有***的热性能,短期可耐260℃,并可在200~240℃下长期使用;其耐热性与PI相当,仅次于F4塑料,这在热固性塑料中也不多见。