日本油墨玻矿增强PPS FZ-3600
Density / Specific Gravity | 1.96 | g/cm | ASTM D792 |
Molding Shrinkage |
|
| ASTM D955 |
Flow | 0.25 | % |
|
Across Flow | 1.0 | % |
|
Water Absorption(24 hr, 23°C) | 0.020 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
Rockwell Hardness |
|
| ASTM D785 |
M-Scale | 100 |
|
|
R-Scale | 121 |
|
|
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 18500 | MPa | ASTM D638 |
Tensile Strength | 125 | MPa | ASTM D638 |
Tensile Elongation(Break) | 0.80 | % | ASTM D638 |
Flexural Modulus | 17500 | MPa | ASTM D790 |
Flexural Strength | 200 | MPa | ASTM D790 |
Flexural Elongation (Break) | 1.3 | % | ASTM D790 |
Compressive Strength | 150 | MPa | ASTM D695 |
Poisson's Ratio | 0.34 |
|
|
Coefficient of Friction3 |
|
| ASTM D1894 |
vs. Steel - Dynamic | 0.35 |
|
|
vs. Steel - Static | 0.35 |
|
|
| Impact | Nominal Value | Unit | Test Method |
Notched Izod Impact | 70 | J/m | ASTM D256 |
Unnotched Izod Impact | 260 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load(1.8 MPa, Unannealed) | 265 | °C | ASTM D648 |
CLTE |
|
| ASTM D696 |
Flow : -30 to 90°C | 1.7E-5 | cm/cm/°C |
|
Transverse : -30 to 90°C | 1.7E-5 | cm/cm/°C |
|
pps的抗拉强度、抗弯强度等性能在工程塑料中属中等水平,而伸长率和冲击强度却很低,因此在受力构件中使用pps通常加入添加剂,如玻纤、碳纤、填料等来增强其力学性能,pps通过这种改性后,主要力学性能,如抗拉性能、抗弯性能、压缩和冲击强度均有大幅度提高,伸长率却有下降,改性后的pps能在长期负荷和热负荷的作用下保持高的力学性能和尺寸稳定性,因而可应用于温度高的受力环境中。