***日本油墨***PPS FZL-4033玻纤PTFE增强
Density / Specific Gravity | 1.68 | g/cm | ASTM D792 |
Molding Shrinkage |
|
| ASTM D955 |
Flow | 0.25 | % |
|
Across Flow | 1.2 | % |
|
Water Absorption(24 hr, 23°C) | 0.020 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
Rockwell Hardness |
|
| ASTM D785 |
M-Scale | 98 |
|
|
R-Scale | 118 |
|
|
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 10000 | MPa | ASTM D638 |
Tensile Strength | 150 | MPa | ASTM D638 |
Tensile Elongation(Break) | 1.6 | % | ASTM D638 |
Flexural Modulus | 9000 | MPa | ASTM D790 |
Flexural Strength | 230 | MPa | ASTM D790 |
Flexural Elongation (Break) | 2.1 | % | ASTM D790 |
Compressive Strength | 180 | MPa | ASTM D695 |
Poisson's Ratio | 0.36 |
|
|
Coefficient of Friction3 |
|
| ASTM D1894 |
vs. Steel - Dynamic | 0.22 |
|
|
vs. Steel - Static | 0.22 |
|
|
| Impact | Nominal Value | Unit | Test Method |
Notched Izod Impact | 75 | J/m | ASTM D256 |
Unnotched Izod Impact | 400 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load(1.8 MPa, Unannealed) | 265 | °C | ASTM D648 |
PPS在负荷下的耐蠕变性好,硬度高;***性高,其1000转时的磨耗量仅为0.04g,填充F4及二硫化钼后还会进一步得到改善;PPS还具有一定的自润性。PPS的机械性能对温度的敏感性能小(3)热学性能:PPS具有***的热性能,短期可耐260℃,并可在200~240℃下长期使用;其耐热性与PI相当,仅次于F4塑料,这在热固性塑料中也不多见。