代理美国SABIC 17%矿物PPO NORYL HS2000X
Density / Specific Gravity | 1.25 | g/cm | ASTM D792 |
Melt Mass-Flow Rate (MFR) |
|
| ASTM D1238 |
280°C/5.0 kg | 7.6 | g/10 min |
|
300°C/5.0 kg | 7.6 | g/10 min |
|
Melt Volume-Flow Rate (MVR) |
|
| *** 1133 |
280°C/5.0 kg | 6.0 | cm/10min |
|
300°C/5.0 kg | 6.0 | cm/10min |
|
Molding Shrinkage - Flow(3.20 mm) | 0.50 to 0.70 | % | Internal Method |
Outdoor Suitability | f1 |
| UL 746C |
| Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus |
|
|
|
--2 | 3650 | MPa | ASTM D638 |
-- | 4000 | MPa | *** 527-2/1 |
Charpy Notched Impact Strength(23°C) | 10 | kJ/m | *** 179/2C |
Notched Izod Impact |
|
|
|
23°C | 130 | J/m | ASTM D256 |
23°C6 | 9.0 | kJ/m | *** 180/1A |
Unnotched Izod Impact(23°C) | 2200 | J/m | ASTM D4812 |
Reverse Notch Izod Impact(3.20 mm) | 810 | J/m | ASTM D256 |
Instrumented Dart Impact(23°C, Total Energy) | 443 | J | ASTM D3763 |