PROPERTIES |
| TYPICAL VALUES | UNITS | TEST METHODS |
---|
MECHANICAL | 1) |
|
|
|
---|
Tensile Stress, yld, Type I, 50 mm/min |
| 53 | MPa | ASTM D638 |
---|
Tensile Strain, brk, Type I, 50 mm/min |
| 50 | % | ASTM D638 |
---|
Flexural Stress, yld, 2.6 mm/min, 100 mm span |
| 81 | MPa | ASTM D790 |
---|
Flexural Modulus, 2.6 mm/min, 100 mm span |
| 2300 | MPa | ASTM D790 |
---|
IMPACT | 1) |
|
|
|
---|
Izod Impact, notched, 23°C |
| 320 | J/m | ASTM D256 |
---|
Izod Impact, notched, -40°C |
| 160 | J/m | ASTM D256 |
---|
Instrumented Dart Impact Energy @ peak, 23°C |
| 53 | J | ASTM D3763 |
---|
Instrumented Dart Impact Energy @ peak, -30°C |
| 25 | J | ASTM D3763 |
---|
THERMAL | 1) |
|
|
|
---|
HDT, 0.45 MPa, 6.4 mm, unannealed |
| 123 | °C | ASTM D648 |
---|
HDT, 1.82 MPa, 6.4 mm, unannealed |
| 121 | °C | ASTM D648 |
---|
CTE, 0°C to 100°C, flow |
| 9.36E-05 | 1/°C | ASTM E831 |
---|
PHYSICAL | 1) |
|
|
|
---|
Specific Gravity |
| 1.05 | - | ASTM D792 |
---|
Water Absorption, (23°C/24hrs) |
| 0.2 | % | ASTM D570 |
---|
Mold Shrinkage, flow, 3.2 mm | 3) | 0.5-0.7 | % | SABIC method |
---|
INJECTION MOLDING | 2) |
|
|
|
---|
Drying Temperature |
| 95-105 | °C |
|
---|
Drying Time |
| 3-4 | Hrs |
|
---|
Drying Time (Cumulative) |
| 8 | Hrs |
|
---|
Maximum Moisture Content |
| 0.02 | % |
|
---|
Melt Temperature |
| 265-295 | °C |
|
---|
Nozzle Temperature |
| 265-295 | °C |
|
---|
Front - Zone 3 Temperature |
| 255-295 | °C |
|
---|
Middle - Zone 2 Temperature |
| 245-290 | °C |
|
---|
Rear - Zone 1 Temperature |
| 230-280 | °C |
|
---|
Mold Temperature |
| 65-95 | °C |
|
---|
Back Pressure |
| 0.3-0.7 | MPa |
|
---|
Screw Speed |
| 20-100 | rpm |
|
---|
Shot to Cylinder Size |
| 30-70 | % |
|
---|
Vent Depth |
| 0.038-0.051 | mm |
|
---|
产品参数
- 否
- 中国
- EM6101
- 注塑
- NORYL EM6101 良好的性能保持/宽温度范围