沙伯基础阻燃高耐热PPE/PS NORYL N300X
Additive |
|
Features | Bromine FreeChlorine FreeFlame RetardantGood Dimensional Stability |
Uses | AppliancesConstruction ApplicationsElectrical/Electronic ApplicationsElectronic DisplaysLawn and Garden EquipmentLighting ApplicationsMedical/Healthcare ApplicationsOutdoor Applications |
Processing Method |
|
Density / Specific Gravity | 1.10 | g/cm | ASTM D792 |
Melt Mass-Flow Rate (MFR)(280°C/5.0 kg) | 7.4 | g/10 min | ASTM D1238 |
Melt Volume-Flow Rate (MVR)(280°C/5.0 kg) | 7.00 | cm/10min | ISO 1133 |
Molding Shrinkage | Internal Method | ||
Across Flow2 | 0.50 to 0.70 | % | |
Flow : 3.20 mm | 0.50 to 0.70 | % | |
Water Absorption(Equilibrium, 23°C) | 0.060 | % | ASTM D570 |
Hardness | Nominal Value | Unit | Test Method |
Rockwell Hardness(R-Scale) | 119 | ASTM D785 |
Notched Izod Impact | |||
-30°C | 55 | J/m | ASTM D256 |
23°C | 190 | J/m | ASTM D256 |
23°C7 | 15 | kJ/m | ISO 180/1A |
Instrumented Dart Impact(23°C, Total Energy) | 54.0 | J | ASTM D3763 |
Thermal | Nominal Value | Unit | Test Method |
Deflection Temperature Under Load | |||
0.45 MPa, Unannealed, 3.20 mm | 155 | °C | ASTM D648 |
0.45 MPa, Unannealed, 4.00 mm, 100 mm Span8 | 156 | °C | ISO 75-2/Be |